· Mnsteels Premium Crusher Wear Parts. All castings go through a cooling phase which takes from 48 hours to 120 hours depending on the thickness of the castings. For example, our C200 plates are about 300 mm thick, so they have to cool down for at least 100 hours. Each casting has a process sheet which lists the related requirements, including .